Parameter   SIR 10
Wallace Rapid Plasticity (Po), Min   30
Plasticity Retention Index (PRI), min %   50
Mooney Viscocity, ML (1'+4') 100 deg C   -
Dirt Retainer on 44 micrometer aperture (max %wt)   0,08
Ash Content, max %wt   0,75
Nitrogen, max %wt   0,60
Volatille matter, max %wt   0,80
Color -
Size -